S460NL执行EN10025标准,是进行正火/正火轧制工艺热处理的低合金钢板,其中N代表的就是正火或者正火轧制,冲击温度为-50°C。
2、S460NL化学成分
C≤0.20,Si≤0.60,Mn1.00~1.70,P≤0.025,S≤0.020,Ni≤0.80,Cr≤0.30,Mo≤0.10,Nb≤0.05,V≤0.20,Ti≤0.05,Al≥0.02,N≤0.025,Cu ≤0.55,。
2、S460NL化学成分
C≤0.20,Si≤0.60,Mn1.00~1.70,P≤0.025,S≤0.020,Ni≤0.80,Cr≤0.30,Mo≤0.10,Nb≤0.05,V≤0.20,Ti≤0.05,Al≥0.02,N≤0.025,Cu ≤0.55,。